Abstract
In this communication, we compare effects of hydrostatic and chemical pressure on the magnetic properties of La0.67Ca0.33(CoxMn1−x)O3 ceramics. For ceramics with x = 0.03, the Curie temperature TC increases under hydrostatic pressure with a slope dTc/dp = +23.4 K/GPa. The saturated magnetization μs does not change with applied hydrostatic pressure. Chemical pressure was induced by substitution of Co for Mn. The substitution from x = 0.03 to x = 0.1 reduces the volume of the elementary cell by about 0.28 %, but TC decreases from 203.4 to 167 K. The saturated magnetization μs is not affected by this substitution.
Original language | English |
---|---|
Pages (from-to) | 12-16 |
Number of pages | 5 |
Journal | High Pressure Research |
Volume | 30 |
Issue number | 1 |
Publication status | Published - Mar 2010 |
Fields of science
- 104005 Electrochemistry
- 104006 Solid state chemistry
- 104014 Surface chemistry
- 104017 Physical chemistry
- 105113 Crystallography
- 105116 Mineralogy
- 503013 Subject didactics of natural sciences
- 204 Chemical Process Engineering
- 204001 Inorganic chemical technology
- 205016 Materials testing
- 210006 Nanotechnology
- 211104 Metallurgy
JKU Focus areas
- Engineering and Natural Sciences (in general)